ASME SA-266 Gr.2 Normalized Tubesheet Forging for Shell & Tube Heat Exchanger
Overview
Yuhong Group Co., Ltd. supplies ASME SA-266 Gr.2 Normalized (Gr.2N) carbon steel tubesheet forgings for shell and tube heat exchangers, pressure vessels, and boiler components. SA-266 Gr.2 is a carbon steel forging specification under ASME Section II Part A, covering components where a wrought, pore-free structure is required rather than plate cut-outs. The normalized (N) condition refines the grain structure and improves through-thickness mechanical uniformity, which matters for thick tubesheets carrying dense tube-hole patterns and tube-to-tubesheet joint loads. The forging is machined to the approved drawing, with tube holes drilled, reamed, and inspected against the specified pitch and tolerance. Tube-to-tubesheet attachment methods include rolling, strength welding, or a combination of both, selected against the tube grade and design pressure.
Material & Mechanical Properties
Chemical Composition (ASME SA-266 Gr.2)
| Element |
Specification range (%) |
| Carbon (C) |
≤ 0.30 |
| Manganese (Mn) |
0.40 – 1.05 |
| Phosphorus (P) |
≤ 0.025 |
| Sulfur (S) |
≤ 0.025 |
| Silicon (Si) |
0.15 – 0.35 |
Mechanical Properties — ASME Specification Basis
The values below are the ASME SA-266 Gr.2 specification requirements. Values for the normalized (Gr.2N) condition are verified against the same specification limits, with heat treatment records confirming the normalized cycle.
| Property |
ASME SA-266 Gr.2 specification |
| Tensile strength |
485 – 655 MPa (70 – 95 ksi) |
| Yield strength, min |
250 MPa (36 ksi) |
| Elongation, min |
20% (in 2 inches) |
| Reduction of area, min |
33% |
| Brinell hardness, max |
Not specified as a rejection limit |
Heat Treatment
All SA-266 Gr.2 forgings are supplied in one of three conditions: annealed, normalized, or normalized and tempered. When tempering is performed, the tempering temperature shall be at a subcritical temperature but not less than 595°C (1100°F). For Gr.2N, the forging is normalized after forging to refine the grain structure, and the heat treatment cycle data is included in the certification package. Quenching and tempering is available only when mutually agreed between manufacturer and purchaser.
High-Temperature Design Basis
For design at elevated temperature, the allowable stress values are taken from ASME Section II for SA-266 Gr.2 at the metal design temperature. The specification does not publish a single maximum use temperature; the practical ceiling is established by the design calculation and the applicable Part D table. For non-severe service, SA-266 Gr.2N tubesheets are commonly applied in the ≤ 427°C range, with the final allowable stress confirmed for the specific design temperature and thickness.
Manufacturing & Inspection Scope
| Stage |
Verification item |
Standard / method |
| Forging |
Grain flow and internal soundness |
Forged from steel ingot or bloom; UT on the raw forging to detect internal discontinuities |
| Heat treatment |
Normalizing cycle |
Furnace chart and cycle record included with certification |
| Machining |
Tube hole pattern, pitch, tubesheet OD/thickness |
Machined to approved drawing; dimensional report issued |
| Tube holes |
Diameter, surface finish, pitch tolerance |
TEMA hole pattern and tolerance requirements |
| Surface examination |
Finished surface integrity |
PT or MT on gasket faces and tube-hole lands as specified |
| Material identity |
Grade confirmation |
PMI on finished forging |
| Certification |
EN 10204 3.1 / 3.2 MTC |
Heat number traceable to chemical and mechanical test results |
Application Envelope
-
Shell and tube heat exchangers: stationary tubesheets for fixed tubesheet (BEM) or U-tube (AEU) bundles, where the tubesheet must resist tube-side pressure, shell-side pressure, and tube-to-tubesheet joint loads simultaneously.
-
Pressure vessel closures: hubbed flat heads, channel covers, and similar pressure-retaining components requiring a forged, weldable carbon steel.
-
Boiler and auxiliary equipment: components within the ASME Section I or Section VIII scope where SA-266 Gr.2N is listed as an acceptable material.
-
Service limitation: SA-266 Gr.2N is a carbon steel forging and is not intended for highly corrosive process fluids without cladding, lining, or a corrosion allowance. For wet H₂S or aggressive chemical service, a stainless steel or alloy tubesheet should be evaluated instead.
QA/QC & Certifications
-
Mill Test Certificate (EN 10204 3.1 or 3.2): traceable to the forging heat number, with chemical analysis and mechanical test results reported against the ASME SA-266 specification.
-
Heat treatment records: furnace charts confirming the normalized cycle, with tempering temperature (where applicable) recorded at ≥ 595°C (1100°F).
-
Non-destructive examination: UT on the forging prior to machining; PT or MT on finished surfaces and tube-hole lands as specified on the purchase order.
-
Dimensional inspection: tube hole diameter, pitch, ligament width, tubesheet thickness, and bolt circle verified against the drawing and TEMA hole-pattern requirements.
-
PMI: positive material identification performed on the finished forging to confirm grade before shipment.
Packaging & Shipping
-
Surface protection: gasket faces and tube-hole lands coated with a rust-preventive compound suitable for marine transit; machined surfaces protected with wooden or plastic covers.
-
Packaging: secured in a plywood case or iron-frame crate, with lifting points marked. Heavy tubesheets are blocked to prevent movement during ocean freight.
-
Documentation: MTC, heat treatment charts, dimensional report, NDT reports, and PMI record sealed in a watertight document holder attached to the crate.
FAQ
-
What does the “N” in SA-266 Gr.2N signify, and why does it matter for a tubesheet?
-
The “N” designates the normalized heat treatment condition.
-
Normalizing refines the grain structure and improves the uniformity of mechanical properties through the thickness, which is relevant for thick tubesheets with dense tube-hole patterns.
-
The normalized condition is verified by furnace chart and mechanical testing from the same heat.
-
What is the maximum tempering temperature requirement?
-
Where tempering is performed after normalizing, the tempering temperature shall be not less than 595°C (1100°F).
-
The tempering temperature is recorded on the heat treatment chart and included in the certification package.
-
Is SA-266 Gr.2N suitable for wet H₂S service?
-
SA-266 Gr.2N is a carbon steel forging and does not carry the alloying elements or hardness controls required for wet H₂S service under NACE MR0175/ISO 15156.
-
For wet H₂S duty, a stainless steel or alloy tubesheet with the appropriate hardness and chemistry should be evaluated against the partial pressure and pH of the process stream.
-
What are the commercial terms?
-
MOQ: 1 piece per size or drawing.
-
Incoterms: FOB, FCA, CIF, or EXW, quoted against the agreed shipment mode and destination.
-
Lead time: approximately 30–60 days after drawing approval, depending on forging procurement, heat treatment cycle, and NDT scope.
Contact