ASTM A335 P22 Alloy Steel Seamless Pipe For High-Pressure Application
Product Overview
ASTM A335 P22 alloy steel seamless pipe is a chromium-molybdenum alloy steel pipe designed for high-temperature service. Commonly known as 2.25Cr-1Mo steel, P22 contains approximately 2.25% chromium and 1% molybdenum, providing material properties suitable for elevated-temperature pressure piping applications.
Chromium contributes to oxidation resistance, while molybdenum supports high-temperature strength and resistance to creep deformation. This alloy composition makes P22 suitable for selected applications in thermal power generation, petrochemical processing, oil refineries, and industrial steam systems.
ASTM A335/A335M covers seamless ferritic alloy-steel pipe intended for high-temperature service. P22 pipes are supplied according to specified chemical composition, heat treatment, mechanical properties, dimensional tolerances, and inspection requirements.
Technical Specifications
| Item |
Description |
| Product Name |
Alloy Steel Seamless Pipe |
| Material Grade |
P22 |
| UNS Designation |
K21590 |
| Common Designation |
2.25Cr-1Mo |
| Material Type |
Chromium-Molybdenum Alloy Steel |
| Standard |
ASTM A335/A335M |
| ASME Standard |
ASME SA335/SA335M, when specified |
| Manufacturing Process |
Seamless |
| Manufacturing Method |
Hot Finished / Cold Drawn |
| Size |
As per customer requirements |
| Outer Diameter |
As per applicable pipe dimensions |
| Wall Thickness |
As per Schedule or customer requirements |
| Length |
Random or specified length |
| Heat Treatment |
Full Annealing, Isothermal Annealing, or Normalizing and Tempering |
| Minimum Tempering Temperature |
675°C for normalizing and tempering |
| Surface Condition |
As agreed |
| Inspection |
Mechanical, dimensional, and applicable nondestructive testing |
| Documentation |
Material Test Certificate (MTC) |
Chemical Composition of ASTM A335 P22
P22 contains chromium and molybdenum as its principal alloying elements. Their controlled composition contributes to the material's performance in elevated-temperature service.
| Element |
Composition (%) |
| Carbon (C) |
0.05–0.15 |
| Manganese (Mn) |
0.30–0.60 |
| Phosphorus (P) |
≤ 0.025 |
| Sulfur (S) |
≤ 0.025 |
| Silicon (Si) |
≤ 0.50 |
| Chromium (Cr) |
1.90–2.60 |
| Molybdenum (Mo) |
0.87–1.13 |
Mechanical Properties
Typical ASTM A335 P22 mechanical requirements at room temperature are listed below.
| Property |
Requirement |
| Tensile Strength |
415–585 MPa |
| Yield Strength (0.2% Offset) |
≥ 205 MPa |
| Elongation |
According to specimen dimensions and orientation |
| Hardness |
According to applicable ASTM requirements |
Mechanical properties should be evaluated against the applicable ASTM A335/A335M edition, pipe dimensions, and test specimen requirements.
Key Characteristics of ASTM A335 P22 Pipe
-
Chromium-Molybdenum Alloy Composition
P22 contains 1.90–2.60% chromium and 0.87–1.13% molybdenum. These alloying elements contribute to its high-temperature material characteristics and distinguish it from conventional carbon steel piping.
-
High-Temperature Strength
Molybdenum contributes to the material's strength at elevated temperatures and resistance to creep deformation. P22 is commonly selected for industrial piping systems operating under elevated-temperature conditions.
The chromium content improves resistance to oxidation compared with conventional carbon steel. This characteristic is relevant to selected high-temperature steam and process piping applications.
-
Heat Treatment Requirements
Heat treatment is important for achieving the required mechanical properties and microstructure. ASTM A335 P22 can be supplied in full-annealed, isothermal-annealed, or normalized-and-tempered conditions, as permitted by the applicable specification.
Heat Treatment of P22 Alloy Steel Pipe
Heat treatment is a critical manufacturing requirement for ASTM A335 P22 seamless pipe.
Typical heat treatment options include:
| Heat Treatment |
Description |
| Full Annealing |
Controlled heating and cooling to achieve the specified material condition |
| Isothermal Annealing |
Heat treatment involving controlled transformation at an intermediate temperature |
| Normalizing and Tempering |
Normalizing followed by tempering to achieve the required mechanical properties |
For normalizing and tempering, the minimum tempering temperature is 675°C (1250°F).
Actual heat treatment parameters, holding times, and cooling procedures must comply with the applicable ASTM A335/A335M edition.
Manufacturing Process
ASTM A335 P22 pipe is manufactured through a seamless production process.
Typical manufacturing and quality control stages include:
-
Alloy steel billet selection and chemical composition verification.
-
Billet heating and piercing.
-
Hot rolling or other applicable seamless pipe forming processes.
-
Heat treatment according to ASTM A335/A335M requirements.
-
Surface conditioning and dimensional finishing.
-
Mechanical testing and dimensional inspection.
-
Applicable nondestructive examination and hydrostatic testing.
-
Final inspection, marking, and preparation of material documentation.
Specific manufacturing methods and inspection capabilities should be confirmed with the manufacturer.
Applications of ASTM A335 P22 Alloy Steel Pipe
Used in selected high-temperature piping systems in thermal power plants, including steam-related piping and pressure equipment.
Applied in high-temperature steam piping and associated industrial pressure systems where chromium-molybdenum alloy steel is specified.
Used in process piping and equipment operating under elevated temperatures.
Applied in selected refinery piping systems, heaters, and high-temperature process lines.
-
Industrial Heating Equipment
Used in selected thermal processing systems and industrial heating installations.
Suitable for specified high-temperature pressure piping applications in industrial energy facilities.
Final material selection should consider operating temperature, pressure, design stress, corrosion conditions, and applicable engineering codes.
ASTM A335 P22 vs. P11
P11 and P22 are both chromium-molybdenum alloy steel grades used in high-temperature applications. Their main difference is the chromium and molybdenum content.
| Comparison |
P11 |
P22 |
| Common Designation |
1.25Cr-0.5Mo |
2.25Cr-1Mo |
| Chromium |
1.00–1.50% |
1.90–2.60% |
| Molybdenum |
0.44–0.65% |
0.87–1.13% |
| Minimum Tensile Strength |
415 MPa |
415 MPa |
| Minimum Yield Strength |
205 MPa |
205 MPa |
| Material Type |
Cr-Mo Alloy Steel |
Cr-Mo Alloy Steel |
| Typical Application |
High-temperature service |
Higher alloy content high-temperature service |
P22 contains higher chromium and molybdenum levels than P11. The choice between these grades depends on design temperature, pressure, allowable stress, service conditions, and project specifications.
ASTM A335 P22 vs. P9
Although P22 and P9 are both chromium-molybdenum alloy steels, they have different alloy compositions and application requirements.
| Comparison |
P22 |
P9 |
| Common Designation |
2.25Cr-1Mo |
9Cr-1Mo |
| Chromium |
1.90–2.60% |
8.00–10.00% |
| Molybdenum |
0.87–1.13% |
0.90–1.10% |
| Minimum Tensile Strength |
415 MPa |
415 MPa |
| Minimum Yield Strength |
205 MPa |
205 MPa |
| Material Category |
Cr-Mo Alloy Steel |
9Cr-1Mo Alloy Steel |
P9 has substantially higher chromium content than P22, while their molybdenum ranges are relatively similar. Material selection should be based on the applicable design requirements and operating environment rather than chromium content alone.
ASTM A335 P22 vs. P91
P22 and P91 are used in high-temperature industrial applications, but their alloy designs and mechanical properties differ.
| Comparison |
P22 |
P91 |
| Material Designation |
2.25Cr-1Mo |
Modified 9Cr-1Mo-V-Nb |
| Chromium |
1.90–2.60% |
8.00–9.50% |
| Molybdenum |
0.87–1.13% |
0.85–1.05% |
| Additional Alloying Elements |
— |
Vanadium, Niobium, Nitrogen |
| Minimum Tensile Strength |
415 MPa |
585 MPa |
| Minimum Yield Strength |
205 MPa |
415 MPa |
| Typical Selection |
Conventional high-temperature service |
More demanding high-temperature service |
P91 provides higher minimum mechanical strength and creep performance in appropriate applications. However, it also requires more stringent fabrication, welding, and heat treatment controls.